Properties
As Cured |
|
|---|---|
| Tensile Strength | 10.7 MPa |
Typical Properties |
|
|---|---|
| Elongation | 320 % |
| Functionality | Fluorosilicone Rubber Compound |
| Hardness | 60 Shore A |
As Cured |
|
|---|---|
| Tensile Strength | 10.7 MPa |
Typical Properties |
|
|---|---|
| Elongation | 320 % |
| Functionality | Fluorosilicone Rubber Compound |
| Hardness | 60 Shore A |