Properties

app.properties.Title

Anti-block No
Slip No

typical.properties.Title

Brittleness Temperature in °C(°F) -52.8 (-63.0)
Density 0.942 g/cm3
ESCR-Environmental Stress Crack Resistance (100% IGEPAL) 6.00 hr - 50˚C (122˚F) F50
Fabrication Method Injection Molding
Functionality Mechanical Performance
Impact Strength in MPa (psi) 90.4 (43.0)
Melt Index ((g/10min @190°C/21.6 kg) (ASTM D1238)) 62
Melt Index (g/10min @190°C/2.16 kg (ASTM D1238)) 62
Structure Type Monolayer, Multilayer
Tensile Elongation at Break, MD 37 %
Tensile Strength Break, MD (ASTM D882) in MPa (psi) 18.6 (2700)
Tensile Strength Yield, MD (ASTM D882) in MPa (psi) 14.5 (2100)