2% Secant Modulus, MD (ASTM D882) in MPa (psi)
|
277 (40200)
|
2% Secant Modulus, TD (ASTM D882) in MPa (psi)
|
330 (47900)
|
Dart Drop Impact (ASTM D1709A) in grams (lbs)
|
410 g
|
Elmendorf Tear Strength, MD (ASTM D1922) in grams (lbs)
|
560 g
|
Elmendorf Tear Strength, TD (ASTM D1922) in grams (lbs)
|
1100 g
|
Fabrication Method
|
Blown Film Extrusion
|
Functionality
|
Mechanical Performance
|
Heat Seal Initiation Temp in °C(°F)
|
120 (248)
|
Melting Point, DSC (Dow Method) in °C(°F)
|
123 (253)
|
Vicat Softening Point in °C(°F)
|
111 (232)
|