2% Secant Modulus, MD (ASTM D882) in MPa (psi)
|
166 (24100)
|
2% Secant Modulus, TD (ASTM D882) in MPa (psi)
|
208 (30200)
|
Dart Drop Impact (ASTM D1709A) in grams (lbs)
|
96 g
|
Elmendorf Tear Strength, MD (ASTM D1922) in grams (lbs)
|
320 g
|
Elmendorf Tear Strength, TD (ASTM D1922) in grams (lbs)
|
190 g
|
Fabrication Method
|
Blown Film Extrusion
|
Functionality
|
Optical Performance, Processing
|
Melting Point, DSC (Dow Method) in °C(°F)
|
108 (226)
|
Puncture Resistance (Dow Method) in joules/cm3 (lbs/in3)
|
3.56 J/cm3 (43 ft lb/in3)
|
Tensile Elongation at Break, MD
|
450 %
|
Tensile Elongation at Break, TD
|
620 %
|
Tensile Strength Break, MD (ASTM D882) in MPa (psi)
|
21.8 (3160)
|
Tensile Strength Break, TD (ASTM D882) in MPa (psi)
|
19.6 (2850)
|
Tensile Strength Yield, MD (ASTM D882) in MPa (psi)
|
11.6 (1690)
|
Tensile Strength Yield, TD (ASTM D882) in MPa (psi)
|
11 (1600)
|
Vicat Softening Point in °C(°F)
|
92.2 (198)
|