Density 0.95 g/cm3
Melt Index (g/10min @190°C/2.16 kg (ASTM D1238)) 17

app.properties.Title

Anti-block No
Component Bicomponent Binder Fibers, Bicomponent Spunbonds, Bicomponent Staple Fibers
Slip No

typical.properties.Title

Enhanced LLDPE No
Fabrication Method Fiber Spinning
Melting Point, DSC (Dow Method) in °C(°F) 130 (266)