性能
关键属性 |
|
---|---|
Density | 0.939 g/cm3 |
Melt Index (g/10min @190°C/2.16 kg (ASTM D1238)) | 15.5 |
应用优势 |
|
---|---|
Anti-block | No |
Slip | No |
典型特性 |
|
---|---|
2% Secant Modulus, MD (ASTM D882) in MPa (psi) | 578 (83800) |
ESCR-Environmental Stress Crack Resistance (100% IGEPAL) | >2000 hr - 100˚C (212˚F) |
Fabrication Method | Blown Film Extrusion |
Functionality | Mechanical Performance |
Tensile Elongation at Break, MD | 630 % |
Tensile Strength Break, MD (ASTM D882) in MPa (psi) | 29.0 (4210) |
Tensile Strength Yield, MD (ASTM D882) in MPa (psi) | 18.0 (2610) |