2% Secant Modulus, MD (ASTM D882) in MPa (psi)
|
190 (27600)
|
2% Secant Modulus, TD (ASTM D882) in MPa (psi)
|
200 (29000)
|
Dart Drop Impact (ASTM D1709A) in grams (lbs)
|
110 g
|
Elmendorf Tear Strength, MD (ASTM D1922) in grams (lbs)
|
500 g
|
Elmendorf Tear Strength, TD (ASTM D1922) in grams (lbs)
|
400 g
|
Fabrication Method
|
Blown Film Extrusion, Cast Film Extrusion
|
Functionality
|
Optical Performance, Processing
|
Tensile Elongation at Break, MD
|
450 %
|
Tensile Elongation at Break, TD
|
650 %
|
Tensile Strength Break, MD (ASTM D882) in MPa (psi)
|
22 (3190)
|
Tensile Strength Break, TD (ASTM D882) in MPa (psi)
|
20 (2900)
|
Tensile Strength Yield, MD (ASTM D882) in MPa (psi)
|
10 (1450)
|
Tensile Strength Yield, TD (ASTM D882) in MPa (psi)
|
11 (1600)
|