性能
关键属性 |
|
|---|---|
| Density | 0.940 g/cm3 |
| Melt Index ((g/10min @190°C/21.6 kg) (ASTM D1238)) | 9.5 |
| Melt Index (g/10min @190°C/2.16 kg (ASTM D1238)) | 0.16 |
应用优势 |
|
|---|---|
| Anti-block | No |
| Slip | No |
典型特性 |
|
|---|---|
| Brittleness Temperature in °C(°F) | < -75 |
| Density Range | .940-.950 |
| Fabrication Method | Pipe Extrusion |
| Tensile Elongation at Break, MD | > 600 % |
| Tensile Elongation at Break, TD | > 600 % |
| Tensile Strength Yield, MD (ASTM D638) in MPa (psi) | > 17.9 (> 2600) |
| Tensile Strength Yield, TD (ASTM D638) in MPa (psi) | > 17.9 (> 2600) |