[{"values":[{"value":"Português do Brasil-ブラジルポルトガル語","languageCode":"pt-br","link":"javascript:void(0);"},{"value":"日本語","languageCode":"ja-jp","link":"javascript:void(0);"},{"value":"中文-中国語(簡体字","languageCode":"zh-cn","link":"javascript:void(0);"},{"value":"English-英語","languageCode":"en-us","link":"javascript:void(0);"}],"label":"BR","default":"pt-br"},{"values":[{"value":"Português do Brasil-ブラジルポルトガル語","languageCode":"pt-br","link":"javascript:void(0);"},{"value":"日本語","languageCode":"ja-jp","link":"javascript:void(0);"},{"value":"中文-中国語(簡体字","languageCode":"zh-cn","link":"javascript:void(0);"},{"value":"English-英語","languageCode":"en-us","link":"javascript:void(0);"}],"label":"JP","default":"ja-jp"},{"values":[{"value":"Português do Brasil-ブラジルポルトガル語","languageCode":"pt-br","link":"javascript:void(0);"},{"value":"日本語","languageCode":"ja-jp","link":"javascript:void(0);"},{"value":"中文-中国語(簡体字","languageCode":"zh-cn","link":"javascript:void(0);"},{"value":"English-英語","languageCode":"en-us","link":"javascript:void(0);"}],"label":"CN","default":"zh-cn"},{"values":[{"value":"Português do Brasil-ブラジルポルトガル語","languageCode":"pt-br","link":"javascript:void(0);"},{"value":"日本語","languageCode":"ja-jp","link":"javascript:void(0);"},{"value":"中文-中国語(簡体字","languageCode":"zh-cn","link":"javascript:void(0);"},{"value":"English-英語","languageCode":"en-us","link":"javascript:void(0);"}],"label":"US","default":"en-us"}]

XUS 81841.27 Experimental Polyethylene Resin

A cast film polyethylene medium density resin designed to improve processing and performance for both breathable and non-breathable backsheet resins in hygiene applications. Main Characteristics - Linear Low Density Polyethylene - Improved processability for cast film - High modulus for downgauged applications

物性

これらの値は一般特性を表すもので、規格ではありません。

  • Anti-block はい いいえ false
  • Dart Drop Impact (ASTM D1709A) in grams (lbs) はい いいえ 27 g
  • Density (ASTM D792) はい いいえ 0.947 g/cm3
  • Elmendorf Tear Strength, MD (ASTM D1922) in grams (lbs) はい いいえ 28 g
  • Elmendorf Tear Strength, TD (ASTM D1922) in grams (lbs) はい いいえ 72 g
  • Gloss (45 degree) はい いいえ 77 %
  • Haze (ASTM D1003) はい いいえ 5.42 %
  • Melt Index (g/10min @190°C/21.6 kg) はい いいえ 6
  • Melting Point, DSC (Dow Method) in °C(°F) はい いいえ 128°C (263°F)
  • Vicat Softening Point in °C(°F) はい いいえ 126°C (259°F)

この製品の有効な安全データシート(SDS)がありません
詳細については当社にお問い合わせください

選択された言語での当該製品の販売規格は見つかりません

XUS 81841.27 Experimental Polyethylene Resin
この製品にはテクニカルデータシートはございません
詳細については当社にお問い合わせください

XUS 81841.27 Experimental Polyethylene Resin


この製品に関する規制データシートはございません


XUS 81841.27 Experimental Polyethylene Resin
この製品で利用可能な代理店オプションについて お問い合わせください